Fast PVA thermal aging
Problem Phenomenon
PVA product aged at 80°C for 7 days, mechanical properties decrease >30%
Cause Analysis
PVA molecular chains break and degrade under thermal oxidation; antioxidant system incomplete, insufficient protection
Solution
1) Improve the antioxidant system 1010+168+DSTDP; 2) Select high molecular weight grade; 3) Add metal deactivator 0.05wt%
Key Takeaway
Thermal aging is caused by thermal oxidation; improving the antioxidant system is the key