PVA hardness too high

Problembeschreibung
PVA product Shore hardness 5-10 degrees higher than target, hard to the touch
Ursachenanalyse
PVA crystallinity on the high side, increased rigidity; too much filler added; cooling too fast, crystallization incomplete but rigidity frozen
Lösung
1) Reduce cooling rate to make crystallization complete and reduce the hard feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to reduce hardness
Wichtigste Erkenntnis
High hardness is caused by crystallization and filler; adjusting cooling and filler are the key
PVAhigh hardnesscrystallinityfiller amountplasticizer