PVA hardness too high

Sorun Belirtisi
PVA product Shore hardness 5-10 degrees higher than target, hard to the touch
Neden Analizi
PVA crystallinity on the high side, increased rigidity; too much filler added; cooling too fast, crystallization incomplete but rigidity frozen
Çözüm
1) Reduce cooling rate to make crystallization complete and reduce the hard feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to reduce hardness
Temel Çıkarım
High hardness is caused by crystallization and filler; adjusting cooling and filler are the key
PVAhigh hardnesscrystallinityfiller amountplasticizer