Large PVA dimensional change with temperature
Problembeschreibung
PVA product dimensions change >2% in the -20 to 60°C range
Ursachenanalyse
PVA thermal expansion coefficient large; crystallinity on the low side causing high dimensional temperature sensitivity; no annealing treatment, residual stress present
Lösung
1) Add rigid filler to reduce the thermal expansion coefficient; 2) Annealing treatment to stabilize dimensions; 3) Select high crystallinity grade to reduce temperature sensitivity
Wichtigste Erkenntnis
Dimensional temperature sensitivity is caused by a large thermal expansion coefficient; adding filler and annealing are the key