Processing Machinery 3 Aufrufe

PVA internal unmelted particles

Problembeschreibung
PVA product interior shows unmelted transparent or translucent particles
Ursachenanalyse
Screw plasticizing capacity insufficient, temperature on the low side; feeding amount too large exceeding the plasticizing capacity; PVA melting temperature on the high side
Lösung
1) Raise processing temperature to ensure full melting; 2) Reduce feeding amount to match the plasticizing capacity; 3) Increase screw mixing section
Wichtigste Erkenntnis
Unmelted particles are caused by insufficient plasticizing; raising temperature and reducing feeding are the key
PVAunmelted particleplasticizing capacityprocessing temperaturescrew mixing