Processing Machinery 5 görüntüleme

PVA internal unmelted particles

Sorun Belirtisi
PVA product interior shows unmelted transparent or translucent particles
Neden Analizi
Screw plasticizing capacity insufficient, temperature on the low side; feeding amount too large exceeding the plasticizing capacity; PVA melting temperature on the high side
Çözüm
1) Raise processing temperature to ensure full melting; 2) Reduce feeding amount to match the plasticizing capacity; 3) Increase screw mixing section
Temel Çıkarım
Unmelted particles are caused by insufficient plasticizing; raising temperature and reducing feeding are the key
PVAunmelted particleplasticizing capacityprocessing temperaturescrew mixing