PVA surface snakeskin pattern
Problembeschreibung
PVA extruded product surface has snakeskin-like irregular texture
Ursachenanalyse
Extrusion temperature on the low side, uneven melt elastic recovery; uneven die temperature distribution
Lösung
1) Raise extrusion temperature to the processing temperature range; 2) Homogenize die temperature ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Wichtigste Erkenntnis
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; raising temperature and reducing speed are the key