Low-temperature performance changes of PA-type materials require evaluation of applicability

Problembeschreibung
Low-temperature performance changes of PA-type materials require evaluation of applicability
Ursachenanalyse
Cellulose acetate butyrate impact strength decreases and brittleness increases at low temperature Dry-state PA low-temperature brittleness is more severe PA12 has good low-temperature resistance (-40°C) but lower temperatures need verification PA66 has high low-temperature rigidity but low impact PA46 low-temperature performance is better than PA66 but still needs evaluation
Lösung
Perform low-temperature impact testing before low-temperature use Conditioning treatment to improve low-temperature toughness PA12 preferred for low-temperature applications PA66 requires toughening modification at low temperature PA46 has good low-temperature rigidity, toughness needs verification
Wichtigste Erkenntnis
PA at low temperature requires impact testing and selection of suitable grades