Mechanical properties, appearance, and dimensions change after aging

Problembeschreibung
Mechanical properties, appearance, and dimensions change after aging
Ursachenanalyse
UV exposure causes cellulose acetate butyrate yellowing and embrittlement (PA type has poor UV resistance) Thermal-oxidative aging, molecular chain breakage, strength decrease Cellulose acetate butyrate absorbs moisture, repeated dry-wet cycling fatigue (PA type) Long-term contact erosion by chemical media Stress relaxation, deformation after long-term loading
Lösung
Add UV absorbers and antioxidants Select cellulose acetate butyrate grades with high weather resistance Control humidity changes in the use environment Evaluate long-term compatibility with chemical media Consider stress relaxation margin in design
Wichtigste Erkenntnis
Long-term aging needs to be addressed from formulation and use environment