Molds & Tooling 3 Aufrufe

Product deforms on demolding or dimensions unstable

Problembeschreibung
The product deforms on demolding or dimensions unstable, related to the cooling time setting
Ursachenanalyse
Cooling time insufficient, product not fully solidified, deformation on demolding Cooling time too long, low production efficiency Uneven cooling, large differences in cooling rates at various parts Unreasonable cooling water channel design Cooling water temperature too high, low cooling efficiency
Lösung
Reasonably set cooling time according to cellulose acetate butyrate and wall thickness Optimize cooling water channels to ensure uniformity Control cooling water temperature at 15-25°C Extend cooling time at thick-walled parts Avoid too short cooling causing deformation
Wichtigste Erkenntnis
Cooling time needs to be reasonably set according to material and wall thickness
cooling timedemoldingsolidificationwater channels