Material Drying 3 Aufrufe

Silver streaks caused by moisture in CEF processing

Problembeschreibung
White silver streaks appear on the surface of the CEF injection molded part
Ursachenanalyse
The raw material contains moisture >0.05%, which vaporizes during high-temperature processing to form bubbles that are stretched into silver streaks; insufficient drying or condensation of water vapor in the hopper
Lösung
1) Dry the raw material at 80°C for 3-4h to a moisture content <0.02%; 2) Increase the back pressure 0.5-1MPa for venting; 3) Reduce the injection speed to avoid air entrapment; 4) Heat the hopper to prevent condensation of water vapor
Wichtigste Erkenntnis
Silver streaks are caused by moisture vaporization and stretching; drying and venting are the main countermeasures
CEF injectionsilver streakmoisture dryingventingback pressure