Extrusion & Post
9 Aufrufe
Bending Deformation of CMC Extruded Profile
Problembeschreibung
CMC extruded profile shows continuous bending after cooling, with deviation >5mm/m
Ursachenanalyse
Uneven cooling of each face of the profile causes differential shrinkage; uneven die outflow velocity makes the wall thicknesses of the profile different; misalignment of haul-off and extrusion centerlines produces lateral force
Lösung
1)Optimize cooling system to ensure uniform cooling of each face; 2)Adjust die to make flow velocity of each wall uniform and wall thickness consistent; 3)Align haul-off and extrusion centerlines; 4)Increase sizing sleeve length for full sizing before cooling
Wichtigste Erkenntnis
Profile bending is caused by uneven cooling and uneven flow velocity; homogenization and alignment are the key to solution
War das hilfreich?
0 Personen fanden dies hilfreich