Extrusion & Post 9 Aufrufe

DSTDP film excessive thermal shrinkage

Problembeschreibung
DSTDP film thermal shrinkage at 80°C >12%, exceeding the 5% dimensional stability requirement
Ursachenanalyse
DSTDP extrusion orientation is released after heating causing large shrinkage; DSTDP thermal expansion coefficient large; film cooling froze a large amount of orientation stress
Lösung
1) Reduce extrusion draw ratio to reduce frozen-in orientation; 2) film annealing treatment at 60-80°C to release orientation stress; 3) add 5-10wt% rigid resin to reduce thermal shrinkage; 4) biaxial stretching process to balance orientation
Wichtigste Erkenntnis
Film thermal shrinkage is caused by frozen-in orientation; reducing draw ratio and annealing treatment are key
DSTDP filmthermal shrinkageorientation releaseannealing treatmentbiaxial stretching