Material Analysis
3 Aufrufe
DSTDP fast UV aging
Problembeschreibung
After 48h UV irradiation, DSTDP mechanical properties decrease >20%, yellowing
Ursachenanalyse
DSTDP molecular chains rapidly degrade by photo-oxidation under UV; surface molecular chains break forming microcracks
Lösung
1) Add UV absorber 0.3-0.5wt% to block UV; 2) add HALS 0.2wt% for radical scavenging; 3) carbon black 2wt% to physically shield UV
Wichtigste Erkenntnis
Fast UV aging is caused by photo-oxidation; UV absorber and HALS are key