Material Analysis
8 visualizaciones
DSTDP fast UV aging
Fenómeno del problema
After 48h UV irradiation, DSTDP mechanical properties decrease >20%, yellowing
Análisis de la causa
DSTDP molecular chains rapidly degrade by photo-oxidation under UV; surface molecular chains break forming microcracks
Solución
1) Add UV absorber 0.3-0.5wt% to block UV; 2) add HALS 0.2wt% for radical scavenging; 3) carbon black 2wt% to physically shield UV
Conclusión clave
Fast UV aging is caused by photo-oxidation; UV absorber and HALS are key
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!