Molds & Tooling 3 Aufrufe

DSTDP internal shrinkage void

Problembeschreibung
DSTDP thick-wall product center shrinkage void diameter 0.5-2mm
Ursachenanalyse
After the thick-wall region cools, the interior shrinks but the surface has already solidified and cannot be fed; holding time insufficient, gate freezes too early
Lösung
1) Extend holding time until the gate is completely frozen; 2) increase gate size to delay freezing; 3) product design to reduce wall thickness difference
Wichtigste Erkenntnis
Shrinkage void is caused by thick-wall shrinkage and insufficient holding; extending holding is key
DSTDPshrinkage voidthick wallholding timegate freezing