Material Analysis 10 Aufrufe

DSTDP low flexural modulus

Problembeschreibung
DSTDP product flexural modulus <20% of the design value
Ursachenanalyse
DSTDP soft, modulus low; filler addition insufficient or interface poor, not playing a reinforcing role; crystallinity on the low side
Lösung
1) Add 10-15wt% rigid filler to increase modulus; 2) nucleating agent to increase crystallinity; 3) select high modulus grades
Wichtigste Erkenntnis
Low flexural modulus is caused by material softness and insufficient filler; adding rigid filler is key
DSTDPflexural modulusrigid fillernucleating agentcrystallinity