문제 현상
DSTDP product flexural modulus <20% of the design value
원인 분석
DSTDP soft, modulus low; filler addition insufficient or interface poor, not playing a reinforcing role; crystallinity on the low side
해결 방법
1) Add 10-15wt% rigid filler to increase modulus; 2) nucleating agent to increase crystallinity; 3) select high modulus grades
핵심 요약
Low flexural modulus is caused by material softness and insufficient filler; adding rigid filler is key