DSTDP internal black specks carbonization

Problembeschreibung
DSTDP product interior shows 0.1-0.5mm black specks, carbonized matter
Ursachenanalyse
DSTDP heated for a long time in barrel dead corner zones and carbonized; carbon buildup at the screw head; raw material impurities
Lösung
1) Lower processing temperature to reduce carbonization; 2) regularly clean screw and barrel; 3) filter raw material to remove impurities
Wichtigste Erkenntnis
Black specks are caused by thermal carbonization and carbon buildup; temperature reduction and regular cleaning are key