Processing Machinery
8 visualizaciones
DSTDP internal black specks carbonization
Fenómeno del problema
DSTDP product interior shows 0.1-0.5mm black specks, carbonized matter
Análisis de la causa
DSTDP heated for a long time in barrel dead corner zones and carbonized; carbon buildup at the screw head; raw material impurities
Solución
1) Lower processing temperature to reduce carbonization; 2) regularly clean screw and barrel; 3) filter raw material to remove impurities
Conclusión clave
Black specks are caused by thermal carbonization and carbon buildup; temperature reduction and regular cleaning are key