Material Analysis 10 Aufrufe

Glass Fibre insufficient tensile strength

Problembeschreibung
Glass Fibre product tensile strength 15-20% below standard value
Ursachenanalyse
Glass Fibre molecular weight too low, strength foundation insufficient; filler interface poor, no reinforcing effect; excessive orientation, longitudinal strong, transverse weak
Lösung
1) Select high molecular weight Glass Fibre grade; 2) filler coupling agent treatment to improve interface; 3) reduce orientation to reduce longitudinal-transverse difference
Wichtigste Erkenntnis
Insufficient tensile strength is caused by molecular weight and poor interface; selecting high MW grade is key
Glass Fibretensile strengthmolecular weightcoupling agentorientation control