Injection Molding 4 Aufrufe

Glass Fibre periodic surface waviness

Problembeschreibung
Glass Fibre product surface has periodic waviness with spacing 5-15mm
Ursachenanalyse
injection speed fluctuates periodically; hydraulic system unstable; screw rotation speed unstable
Lösung
1) overhaul injection system to stabilize pressure and speed; 2) replace hydraulic drive with servo motor drive; 3) PID control to stabilize injection parameters
Wichtigste Erkenntnis
waviness is caused by unstable injection; equipment overhaul and PID control are key
Glass Fibre surface waviness injection stability equipment overhaul PID control