Material Drying 3 Aufrufe

Glass Fibre internal voids

Problembeschreibung
Glass Fibre products have 1-3mm voids inside, concentrated at the thick-wall center
Ursachenanalyse
insufficient holding, thick-wall center not compacted; gas entrapment cannot be vented; moisture in raw material vaporizes
Lösung
1) increase holding pressure 60-80MPa for full compaction; 2) increase mold venting; 3) fully dry the raw material
Wichtigste Erkenntnis
internal voids are caused by insufficient holding and gas entrapment; high holding pressure and venting are key
Glass Fibre internal voids holding pressure mold venting raw '2079851475616104451