Extrusion & Post 9 Aufrufe

MP extruded film transverse waviness

Problembeschreibung
MP extruded film surface has transverse periodic waviness, wavelength 5-10mm
Ursachenanalyse
haul-off roller vibration or unstable speed producing periodic stretching variation; cooling roller eccentricity or non-round surface causing periodic contact pressure variation
Lösung
1) overhaul the haul-off roller to eliminate vibration; 2) true the cooling roller, eccentricity <0.02mm; 3) install a pressure stabilizing device on the extruder to eliminate pressure fluctuation; 4) stable control of haul-off speed ±0.5%
Wichtigste Erkenntnis
transverse waviness is caused by haul-off vibration and roller eccentricity; equipment overhaul and stable control are key
MP film transverse waviness haul-off vibration cooling roller eccentricity pressure stabilizing device