Problembeschreibung
MP product tensile strength 15-20% below the standard value
Ursachenanalyse
MP molecular weight low, strength foundation insufficient; filler interface poor, no reinforcing effect; excessive orientation, strong longitudinally weak transversely
Lösung
1) select a high molecular weight MP grade; 2) treat filler with coupling agent to improve the interface; 3) reduce orientation to reduce the longitudinal-transverse difference
Wichtigste Erkenntnis
insufficient tensile strength is caused by molecular weight and poor interface; selecting a high MW grade is key