Material Analysis
15 visualizaciones
MP insufficient tensile strength
Fenómeno del problema
MP product tensile strength 15-20% below the standard value
Análisis de la causa
MP molecular weight low, strength foundation insufficient; filler interface poor, no reinforcing effect; excessive orientation, strong longitudinally weak transversely
Solución
1) select a high molecular weight MP grade; 2) treat filler with coupling agent to improve the interface; 3) reduce orientation to reduce the longitudinal-transverse difference
Conclusión clave
insufficient tensile strength is caused by molecular weight and poor interface; selecting a high MW grade is key
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!