Material Drying
3 Aufrufe
Bubble Problem in Compression Molding of PAK Special Engineering Plastic
Problembeschreibung
Polyacrylate ketone PAK shows bubble during compression '2079851475616104453ing at 240-300°C.
Ursachenanalyse
Improper control in the aspect of PAK high-temperature drying).
Lösung
Increase the mold temperature.
Wichtigste Erkenntnis
PAK high-temperature processing requires precise control.