PB polybutene-1 poor welding problem in pipe extrusion
Problembeschreibung
Polybutene-1 PB exhibits poor welding during pipe extrusion processing at 180-230°C.
Ursachenanalyse
PB processing temperature is the key factor.
Lösung
Nucleating agent addition.
Wichtigste Erkenntnis
PB pressure pipes need to control crystal form transition.