Extrusion & Post 9 Aufrufe

The low peel strength problem of PBAK acrylate type in coating

Problembeschreibung
Polybutyl acrylate-type PBAK exhibited low peel strength during coating processing at 80-150°C.
Ursachenanalyse
Improper crosslinking degree of PBAK caused the problem.
Lösung
Control crosslinking.
Wichtigste Erkenntnis
PBAK for coating and adhesive applications requires fine formulation design.
PBAKacrylatelow peel strengthcoatingemulsion polymerization