Material Drying
3 Aufrufe
PBN surface roughness Problem in Extrusion Processing
Problembeschreibung
Polybutylene naphthalate PBN exhibits surface roughness in extrusion processing at 270-300°C.
Ursachenanalyse
Under high-temperature processing at 270-300°C, hydrolysis causes the problem.
Lösung
Solve by nitrogen protection.
Wichtigste Erkenntnis
PBN ultra-high-temperature processing requires comprehensive protection.