Low crystallinity problem of PBS biodegradable material in spinning
Problembeschreibung
Polybutylene succinate PBS shows low crystallinity in spinning processing at 140-200°C.
Ursachenanalyse
Caused by poor thermal stability of PBS and abnormal flow.
Lösung
Improved by shortening the residence time.
Wichtigste Erkenntnis
The degradation characteristics of PBS require gentle processing.