PBS biodegradable material mechanical property decline problem in film blowing
Problembeschreibung
Polybutylene succinate (PBS) exhibits mechanical property decline during film blowing processing at 140-200°C.
Ursachenanalyse
Caused by poor thermal stability and fast degradation of PBS.
Lösung
Improve by sufficient drying.
Wichtigste Erkenntnis
The degradation characteristics of PBS require mild processing.