Material Drying
3 Aufrufe
Control of appearance abnormality in PEOX cast film packaging
Problembeschreibung
During PEOX cast film production of packaging, the problem of not up to standard appearance occurs.
Ursachenanalyse
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.3% exceeding the standard, and excessively long residence time.
Lösung
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Wichtigste Erkenntnis
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!