Material Drying
3 Aufrufe
Control of strength abnormality in PEOX calendering textiles
Problembeschreibung
During PEOX calendering production of textiles, the problem of not up to standard strength occurs.
Ursachenanalyse
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.3% exceeding the standard, and shear heat accumulation.
Lösung
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Wichtigste Erkenntnis
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
War das hilfreich?
0 Personen fanden dies hilfreich