Problembeschreibung
During PEOX '2079851475616104452 production of packaging, the problem of unstable transparency occurs.
Ursachenanalyse
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.3% exceeding the standard, and shear heat accumulation.
Lösung
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and strengthen cooling.
Wichtigste Erkenntnis
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.