Material Drying 3 Aufrufe

Control of demolding abnormality in PEOX cast film packaging

Problembeschreibung
During PEOX cast film production of packaging, the problem of uneven demolding occurs.
Ursachenanalyse
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.1% exceeding the standard, and excessively long residence time.
Lösung
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and strengthen cooling.
Wichtigste Erkenntnis
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.