Material Drying 3 Aufrufe

Internal pores in PPS products

Problembeschreibung
Internal voids appear in PPS products affecting sealing and strength.
Ursachenanalyse
Trace moisture or volatiles in PPS material produce gas; insufficient holding pressure.
Lösung
Dry at 150°C/3-4h; increase holding pressure and time; optimize venting.
Wichtigste Erkenntnis
PPS pores seriously affect the reliability of sealing parts.