Material Drying 3 Aufrufe

PPSU long-term hot water aging

Problembeschreibung
After long-term immersion in 95°C hot water, the mechanical properties of PPSU decline.
Ursachenanalyse
Although PPSU is hydrolysis resistant, slow hydrolysis still occurs under ultra-long-term high-temperature water.
Lösung
Consider hot water aging in service life assessment.
Wichtigste Erkenntnis
PPSU long-term hot water performance needs verification.