6 Aufrufe
Processing temperature too low, poor plasticization
Problembeschreibung
Below 100C, plasticization is insufficient and the surface is rough
Ursachenanalyse
Low temperature, not fully melted, insufficient plasticization
Lösung
Raise to a reasonable range of 100-180C
Wichtigste Erkenntnis
The processing temperature window determines plasticization