Molding Process
5 views
Processing temperature too low, poor plasticization
Problem Phenomenon
Below 100C, plasticization is insufficient and the surface is rough
Cause Analysis
Low temperature, not fully melted, insufficient plasticization
Solution
Raise to a reasonable range of 100-180C
Key Takeaway
The processing temperature window determines plasticization
Was this helpful?
0 people found this helpful