Molding Process 11 views

Incomplete thermal imidization

Problem Phenomenon
The imidization degree of PI is lower than the target value and performance is substandard
Cause Analysis
Final heat treatment temperature not high enough or time insufficient; PAA film/product too thick, internal temperature uneven
Solution
Ensure the final treatment temperature is ≥300°C and hold for a sufficient time; confirm the imidization characteristic peaks by IR spectroscopy (1780/1720/1380 cm⁻¹); control the sample thickness
Key Takeaway
The imidization degree (imidization rate) determines the final performance of PI
imidization degree300°CIR spectroscopytreatment time