Extrusion & Post
5 Aufrufe
POE dimension changes greatly with temperature
Problembeschreibung
POE product dimension changes >2% in the range -20 to 60°C
Ursachenanalyse
POE thermal expansion coefficient large; crystallinity low causing high dimensional temperature sensitivity; no annealing treatment, residual stress present
Lösung
1) Add rigid filler to reduce thermal expansion coefficient; 2) Annealing treatment to stabilize dimensions; 3) Select high crystallinity grade to reduce temperature sensitivity
Wichtigste Erkenntnis
Dimensional temperature sensitivity is caused by large thermal expansion coefficient; adding filler and annealing are key