POE and ABS blend delamination cracking
Problembeschreibung
POE/ABS delaminates along the interface under bending
Ursachenanalyse
POE and ABS polarity completely different, compatibility extremely poor
Lösung
1) POE-g-MAH 3-5wt%; 2) POE≤10wt%; 3) MBS replacing POE to toughen ABS
Wichtigste Erkenntnis
POE/ABS polarity difference requires compatibilizer or changing the toughener