Molding Process 6 Aufrufe

Internal shrinkage porosity in SIS thick-walled products

Problembeschreibung
Center of thick-walled part is porous or has voids
Ursachenanalyse
Center cools slowly, feeding channel solidifies too early
Lösung
Optimize gate position and size, extend holding pressure, increase pressure
Wichtigste Erkenntnis
Internal quality of thick-walled parts is a technical difficulty
SIS shrinkage porosity

War das hilfreich?