Molding Process
3 visualizações
Internal shrinkage porosity in SIS thick-walled products
Fenómeno do problema
Center of thick-walled part is porous or has voids
Análise das causas
Center cools slowly, feeding channel solidifies too early
Solução
Optimize gate position and size, extend holding pressure, increase pressure
Conclusão principal
Internal quality of thick-walled parts is a technical difficulty
Isto foi útil?
0 pessoas acharam isto útil