Molding Process
6 Aufrufe
High porosity of sintered parts
Problembeschreibung
Porosity of sintered molded parts exceeds the standard
Ursachenanalyse
Low powder bulk density, insufficient sintering temperature and holding
Lösung
Two-stage sintering: 200-230C degassing + 260-280C densification
Wichtigste Erkenntnis
Densification sintering is a technical difficulty