Molding Process
5 views
High porosity of sintered parts
Problem Phenomenon
Porosity of sintered molded parts exceeds the standard
Cause Analysis
Low powder bulk density, insufficient sintering temperature and holding
Solution
Two-stage sintering: 200-230C degassing + 260-280C densification
Key Takeaway
Densification sintering is a technical difficulty
Was this helpful?
0 people found this helpful