Extrusion & Post
3 Aufrufe
Poor printability of low density polyethylene film
Problembeschreibung
Poor ink adhesion on the film surface, printed patterns fall off or become blurred.
Poor printability affects product appearance and product quality in printed packaging film.
Ursachenanalyse
(1) Low surface energy of low density polyethylene (<32dyn/cm), poor ink wettability
(2) Insufficient film surface treatment (inadequate corona treatment)
(3) Exudates on film surface (slip agent, anti-blocking agent migration)
(4) Ink and film mismatch
(5) Improper printing environment humidity
Lösung
(1) Perform corona treatment, increase film surface tension to 38-42dyn/cm
(2) Control corona treatment power and time, ensure uniform treatment
(3) Control additive dosage, avoid excessive exudation
(4) Select ink types matching the film
(5) Control printing environment humidity at 50-60%
Wichtigste Erkenntnis
Poor printability is caused by low surface energy; ink adhesion needs to be improved by increasing surface tension through corona treatment.
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!