Extrusion & Post 3 Aufrufe

Haul-off speed mismatch of low density polyethylene extruded products

Problembeschreibung
Extrudate thickness is uneven; when haul-off is too fast the product becomes thinner and narrower, when haul-off is too slow the product becomes thicker and wider. Mismatch between haul-off speed and extrusion speed causes product dimensional deviation.
Ursachenanalyse
(1) Haul-off speed setting mismatched with extrusion speed (2) Haul-off slipping, actual haul-off speed unstable (3) Haul-off clamping force insufficient or excessive (4) Extrusion speed fluctuation makes haul-off synchronization difficult (5) Slow response of haul-off control system
Lösung
(1) Adjust haul-off speed to match extrusion speed, determine synchronous speed by weighing method (2) Check haul-off tracks or rollers, ensure no slipping, replace clamping pads when necessary (3) Adjust haul-off clamping force, ensure uniform clamping without damaging the product (4) Stabilize extrusion speed, reduce fluctuation (5) Upgrade the haul-off control system, improve response speed and accuracy
Wichtigste Erkenntnis
Haul-off speed mismatch needs to be solved by precisely adjusting haul-off parameters and ensuring haul-off stability.
haul-off speedspeed matchinghaul-off slippingclamping forcehaul-off control