Injection Molding 10 Aufrufe

Insufficient filling of PAR '2079851475616104452 (short shot)

Problembeschreibung
The cavity is not completely filled and the product is short of material.
Ursachenanalyse
The PAR melt viscosity is high, and the flowability is still limited at a processing temperature of around 300°C; the injection pressure and speed are insufficient.
Lösung
Raise the melt temperature to 300-320°C; increase the injection pressure and speed; enlarge the gate and runner.
Wichtigste Erkenntnis
The high viscosity of PAR is the main cause of short shot.
PARshort shothigh viscosityprocessing temperaturegate